Polypropylene filler described in this standard is of non-hygroscopic and mainly used during the assembly of insulated cores to fill the space between them in order to make the assembled core if needed round shape.
High Tensile Strength Without Joint;
100% Virgin PP;
Sample Free;
Light Weight.
Dia
[mm] |
Denier
[D] |
Linear Density
[g/m] |
Breaking Strength
[N] |
Elongation
[%] |
Twist
[RPM] |
Tube & Bobbin Size |
Φ1.0 | 8000 | 0.8±5% | ≥20 | ≥12 | Twisted | A |
Φ1.5 | 12000 | 1.2±5% | ≥30 | ≥12 | Twisted | A |
Φ2.0 | 16000 | 1.8±5% | ≥40 | ≥12 | Un-Twisted | A |
Φ2.5 | 24000 | 2.6±5% | ≥60 | ≥12 | Un-Twisted | A |
Φ3.0 | 32000 | 3.4±5% | ≥80 | ≥12 | Un-Twisted | A |
Φ3.5 | 38000 | 4.2±5% | ≥100 | ≥12 | Un-Twisted | A |
Φ4.0 | 45000 | 5.1±5% | ≥120 | ≥12 | Un-Twisted | A |
Φ5.0 | 72000 | 8.0±5% | ≥180 | ≥12 | Un-Twisted | B |
Φ6.0 | 100000 | 11.4±5% | ≥240 | ≥12 | Un-Twisted | B |
Φ7.0 | 135000 | 15.0±5% | ≥300 | ≥12 | Un-Twisted | B |
Φ8.0 | 180000 | 19.0±5% | ≥ 360 | ≥12 | Un-Twisted | C |
Φ9.0 | 270000 | 30.0±8% | ≥450 | ≥12 | Un-Twisted | C |
Φ10.0 | 360000 | 40.0±8% | ≥600 | ≥12 | Un-Twisted | C |
Φ12.0 | 450000 | 51.0±8% | ≥800 | ≥12 | Un-Twisted | C |